Greetings to all subscribers and visitors to the channel made for those who have decided to develop their own manual arc welding. Today I want to show you how I had to perform welding repairs muffler with his old Seven (2107), namely part of the silencer, called the people in your pants!
After removal and inspection, it was found that this part of the muffler burnt in many places, there are two options, the purchase of a new or independent repair welding, of course, in my case it's the second option, otherwise why I welder worth?
Problem areas I obstuchal hammer for a clearer picture of the problem with places of burnout, and cleaned up the grinder. Since the burned-out place was pretty much, I decided to completely circumnavigate the part of the receiving tube (pants) sheet metal 2 mm thick.
Welded seams will be at the factory, which have a good thickness, it is necessary to make only two blanks in the form of a parallelepiped (barely wrote!), I measured the dimensions of the problem areas, and arbitrarily added to these sizes of 50mm (except height) then the excess srezh.
Cut the size of the box 2 and tried to muffle, normally happened.
Friends, many more pictures and descriptions, so I decided to split this topic into 2 parts, if interested, the second part will be released a few days ago.
That would be so!